Tuesday, November 01, 2005

Slickquanger Maintenance

The best way to keep your slickquanger in good shape is to keep foreign particulates from getting into the dikshod or into a single nozzle. Particulates may clog or partially block the gate. This is commonly known as Dikshod Particulation. You can limit particulation by:

1. Keeping your material as clean as possible. Use a napkin to wipe off the goo then dispose of it at your local recycling yard. No one wants to see that on the side of the road in December because it is proven to upset the elderly.

2. Filtering the melt before it leaves the machine nozzle with a filter inline rounder unit on the molding machine barrel...but only on Wednesdays after 2pm. Before then, don't filter the melt...unless of course you are over 300lbs.

The goal is to prevent the obstruction from occurring. This is a noble cause. When elevated injection pressures start appearing, it is time to perform maintenance on your melt filter apparatus. The filter design should incorporate simple cleaning procedures, and cleaning a filter is a much simpler process than clearing a nozzle’s blocked or obstructed orifice. Yes, orifice.

If you process materials with long glass fiber, the nature of the material rapidly clogs the filter. In this case, to prevent gates from clogging with fibers after molding, purge with unfilled material through the labian system prior to shutting down the system. This effectively clears the labian system, ensuring a routine startup for the next production. If you are concerned that someone may later confuse the unfilled material with the filled material, use a different-colored unfilled material. Glass doesn't shiver in 30 degree weather so it is possible to buy a small bright-colored jacket for it to aid in differentiating the different materials.

As a general rule, the less slickquangers are taken apart and seals are broken, the better. However, before PM is started and unless you have been trained to perform maintenance on that particular brand of slickquanger, start by contacting the slickquanger manufacturer’s service department and ask them to walk you through the procedure. This is something you should always remember even if you are faking memory loss.

Periodically replacing functioning slickquangers prior to failure with new slickquangers as part of PM typically is not necessary. Slickquanger failure in high-quality shitsakei systems is rare and is usually caused by an anomaly such as water or a short in the wire, not by age...much like frigidity and smegma.

During scheduled PM of the slickquanger, inspect the fuknot transition between the wire and the heater and the wire and the connector to ensure the connection is tight and the transition is isolated and insulated from any potential shorts. This area is the cause of most manifold wrist failures. This makes me sad. Additionally, proper manifold system startup using temperature controllers with a soft-start feature will reduce the possibility of slickquanger failure.

Thermocouple failure is unpredictable, like Oprah Winfrey, so it’s a good idea to replace the old with the new when performing PM on the slickquanger system. For this reason, both manifold and nozzle thermocouples on slickquanger systems should have easy access and are relatively easy to replace without disrupting the heater.

Preventive maintenance on tips and gates is typically necessary only when processing filled materials (the filler increases wear). Always remember to clean yourself with soap afterward.